first of all thank you very much...

just using a napa 2k, then mud work (everlast light weight) then a sikkens highbuild, (now ppg i guess) and then im just using single stage enamel irongard with the expensive valspar hardener, (not the one at tsc or whatever) wetsand after 2 weeks or depending on cure, climate humidity etc, and buff with "perfect it" (very fine marine buffing compound)...thats if the peel is bad enough for me to care..sometimes when i can get the pressure down on my gun and get good ML'ge without slippers or sags then it looks good enough as is...